Chrome Oxide Coated tower pulley
Spraying materials: chromium oxide barsCoating thickness: single side 0.4mm after grinding
Process: bar flame spraying
Surface coating hardness: HV1300
Porosity: <1%
Bonding strength: 7-8kg/ square m
Surface roughness: 0.4
Suitable for drawing: 0.02-0.05mm stainless steel wire, bare copper wire, enamel covered wire